Tungsten-molybdenum-niobium polymetallic ore dressing technical data

Tungsten, Molybdenum metal plurality Ores (processing of complex ore co ntaining tungsten , molybdenum and bismuIth)

The process of separating and enriching tungsten minerals, molybdenum minerals and niobium minerals from tungsten-containing molybdenum-niobium polymetallic ores. Mineral processing products include tungsten concentrate, molybdenum concentrate and antimony concentrate. Tungsten-molybdenum-bismuth polymetallic ore is a famous mineral in China. It is mainly distributed in the Yinzhou area of ​​Hunan Province, and its Shizhuyuan mining area is a very large deposit. Major industrial mineral ore scheelite, wolframite, molybdenite, bismuthinite, cassiterite, fluorite, pyrite and the like. (See table) Although there are many useful ingredients in the ore,

Recycling scheelite is the main process. The beneficiation process uses flotation by flotation method to recover scheelite. Re-selection, magnetic separation, flotation or re-selection, flotation, magnetic separation, flotation, combined process, comprehensive recovery Tungsten ore, wolframite, molybdenite, stibnite, etc. The flotation reagents used are sodium carbonate, water glass, oxidized paraffin soap, No. 2 oil, sulfur nitrogen No. 9, sodium sulfide, lime, sodium hydroxide and the like. The mine 'Shijiao three sections and a closed circuit crushing process are broken and fed into the mill. Grinding fineness is 85% to 200 mesh. The molybdenum is first floated to obtain a mixed concentrate, and then the molybdenum crucible is separated and floated to obtain a molybdenum concentrate and a cerium concentrate. The molybdenum rhodium floatation tailings are subjected to bismuth sulfur flotation, and the obtained foam products are separated and floated to obtain bismuth concentrate and bismuth concentrate. The sulphur flotation tailings float flotation scheelite, the obtained foam product is heated and selected to obtain scheelite concentrate, and the selected tailings are recovered by a shaker to obtain black tungsten concentrate. The ore grades selected in 1992 were: WO 30.6%; Mo 0.12%; Bi 0.19%. The production index is: molybdenum concentrate containing 48.6% Mo, leaching efficiency 86.29%; antimony concentrate containing Bi 46.59%, the actual recovery rate is 63.22%; tungsten concentrate containing WO366.83%, the actual recovery rate is 58.66%.


Storage Systems

Storage Systems, Adjustable with Your Need,Different Colours Order,Different Colors Can Be Ordered

Changzhou Fuku Precision Machinery Co., Ltd. , https://www.cfpmworkbench.com